Original Research Paper Physics

Effect on particle size and microstrain due to Iron doping on ZnO nanoparticle prepared by wet chemical method.

Anup Kr Kalita *Dr. Sanjib Karmakar

Abstract

<p><p>&lt;p&gt;&amp;lt;p&amp;gt;&amp;amp;nbsp;Iron (Fe) deposited Zinc oxide (ZnO) thin films were successfully deposited by Chemical Bath Deposition (CBD) method with Zinc Acetate Dihydrate as inorganic precursor and Iron Chloride (FeCl3) as dopant. Thin films are prepared for 0.1M, 0.05M and 0.025M doping concentration at room temperature (RT). The films were analyzed by X&amp;amp;ndash;Ray Diffraction (XRD). Using XRD microstrain and particle sizes are calculated at different doping concentration at RT. It is found that as doping concentration increases particle size as well as microstrain increases&amp;lt;/p&amp;gt;&lt;/p&gt;</p></p>

Keywords: Microstrain, Particle size, Scherrer’s equation, Chemical bath deposition