Original Research Paper Engineering

Flexural Behavior of Tbsfrc Subjected to Sustained Elevated Temperature

Dr Deepa A Sinha

Abstract

A detailed investigation is made to study the flexural behaviour of steel fibre reinforced concrete with ternary
blends on the beam specimen when subjected to sustained elevated temperature of 200oC, 400oC, 600oC,
800oC and 1000oC for 3 hours and then allowed to cool. The mix design was carried out for M30 grade concrete which
yielded a proportion of 1:1.86: 2.41 with a w/c ratio of 0.45. Before mixing, 30% of cement was replaced by (FA + SF) or
(FA+GGBFS) or (FA+MK) according to the proportions such as (0+0), (30+0), (25+5), (20+10), (15+15), (10+20), (5+25) and
(0+30) respectively. It has been found that the TBSFRC containing (FA+GGBFS) and (FA+MK) offer higher resistance to
sustained elevated temperatures upto 600oC and 800oC, where as the blend containing (FA+SF) offers resistance only upto
400oC.

Keywords: Flexural strength, ternary blended steel fibre reinforced concrete, fly ash, silica fume, metakaolin, ground granulated blast furnace slag