Original Research Paper Science

Optimisation fabrication of butyl methacrylate monoliths

Eman Alzahrani

Abstract

In this study, a butyl methacrylate–co–ethylene dimethacrylate (BuMA–co–EDMA) monolith was synthesised
using UV–initiated polymerization. The effect of the energy of the UV light (254 and 365 nm), and the
time of exposure to the UV light (8–22 min) on fabrication of the organic polymer monolith were investigated. The
results of this investigation showed that the most suitable wavelength for the photoinitiated polymerisation reaction
in this study was 365 nm. In addition, the finding of this study suggests that the optimum time of exposure to the UV
light in order to prepare a porous rigid monolith was 20 min. Control of the porous properties of the organic polymer
monolith was optimised by adjusting the composition of the porogenic solvents. In this study, eight different binary
porogenic solvent systems containing 50 % of main solvent (MeOH) and 50 % of co–porogen (EtOH, ACN, chloroform,
hexane, tetrahydrofuran, 1–propanol, ethyl acetate, and cyclohexanol) were studied. The characterisation of the bed
structures of the fabricated monoliths was carried out by SEM analysis, BET model, and measuring the porosity and
permeability of the monoliths. The results of this investigation show that the optimal binary porogenic solvent system
to prepare the poly (BuMA–co–EDMA) monolith was MeOH/EtOH, which offers high porosity and permeability. In addition,
this study found that replacing EtOH with 1–propanol enables the fabrication of the organic polymer monolith
with a higher surface area (56.89 m2 g–1).

Keywords: organic monolith, butyl methacrylate, progenic solvent system